My car is a 2002 SV. I started having blisters popping up on the rear aluminum panel in the area of spare tire. Has anyone had this issue, and if so what did you do to solve the problem.

Posted

No, on brass or copper in the general area, maybe 15 feet away I have some copper tubing. Blisters started last year, treated by sanding and brushing with new stainless steel brush and then epoxy primer then paint/clear coat. Paint supplier said that epoxy would work better than zinc chrome-mate?

Posted

If you have some poor grounds in that area (tail or licence plate lights?) you may have stray currents 'roaming about' looking for a better ground. Any electrical systems performing oddly? I have had similar experiences in a marine environment with blistering caused by galvanic action and in that case epoxy primers performed worse than traditional primers. The real solution lay in finding the source of the currents, whether electrical or galvanic.

Posted
No, on brass or copper in the general area, maybe 15 feet away I have some copper tubing. Blisters started last year, treated by sanding and brushing with new stainless steel brush and then epoxy primer then paint/clear coat. Paint supplier said that epoxy would work better than zinc chrome-mate?

 

Zinc Chromate is an excellent primer for aluminum. Sticks well and good at corrosion protection. It's getting hard to fine because the EPA hates it for good reason. Very toxic if you eat it. Sounds like it's not galvanic corrosion.

Dan

Posted

I know Magnus Feuer (administrator of the California Caterham Club web forum) had the same thing with his SV of similar vintage. Might have been a manufacturing flaw, maybe insufficient etching of the aluminum.

Posted

I guess it’s possible that I have a partial grounding issue, but all the lights are functioning well? I could remove the grounding wires and clean and reattach just as a preventive precaution. I know Ford had issues with the Mustang hood due to contamination of iron oxide causing blistering. Maybe my car was poorly prep at factory in this area causing the corrosion? I would like to chat with Magnus about his issues and resolutions!

Posted

Inadequate grounding can cause very severe corrosion damage.

 

You should share a picture. Might be atmospheric corrosion still....... but hard to believe it'd be crevice corrosion.

Posted

That thought was running through my mind last night. My car has the master kill switch on LH side of bulkhead so all voltage is off?

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now
×
×
  • Create New...